PropertyZircadyne 702 (UNS R60702)Zircadyne 705 (UNS R60705)Difference
Yield strength128.9 MPa190.2 MPa+48%
Tensile strength200.6 MPa299.7 MPa+49%
Elongation49 %29 %-41%
Elastic modulus80,700 MPa81,000 MPa0%
Shear modulus36,200 MPa34,500 MPa-5%
Poisson ratio0.350.33-6%
Density6,510 kg/m³6,640 kg/m³+2%
Thermal conductivity22 W/m·K17.1 W/m·K-22%
Specific heat284.7 J/kg·K280.5 J/kg·K-1%
Coefficient of thermal expansion0.000007 1/K0.000006 1/K-18%
Melting point1,852 °C1,840 °C-1%

Difference is Zircadyne 705 (UNS R60705) relative to Zircadyne 702 (UNS R60702). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Zircadyne 702 (UNS R60702)
grade
R60702
standard
ASTM B551 / B523 / B493 / B550 / B658
heat treatment
Annealed
Zircadyne 705 (UNS R60705)
grade
R60705
standard
ASTM B551 / B523 / B493 / B550 / B658
heat treatment
Annealed