Ti CP Grade 2 (CP-2) Extruded Bar/Shape Annealed vs Ti CP Grade 3 (CP-3) Sheet Annealed

Property comparison of Ti CP Grade 2 (CP-2) Extruded Bar/Shape Annealed and Ti CP Grade 3 (CP-3) Sheet Annealed, both titanium alloy.

Titanium Alloy5 compared properties
PropertyTi CP Grade 2 (CP-2) Extruded Bar/Shape AnnealedTi CP Grade 3 (CP-3) Sheet AnnealedDifference
Yield strength275.8 MPa275.8 MPa0%
Tensile strength344.7 MPa344.7 MPa0%
Elastic modulus106,869 MPa106,869 MPa0%
Shear modulus44,816 MPa44,816 MPa0%
Density4,512 kg/m³4,512 kg/m³0%

Difference is Ti CP Grade 3 (CP-3) Sheet Annealed relative to Ti CP Grade 2 (CP-2) Extruded Bar/Shape Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Ti CP Grade 2 (CP-2) Extruded Bar/Shape Annealed
grade
Ti CP Grade 2
standard
MIL-HDBK-5J
heat treatment
Annealed
Ti CP Grade 3 (CP-3) Sheet Annealed
grade
Ti CP Grade 3
standard
MIL-HDBK-5J
heat treatment
Annealed