| Property | Ti-7Al-4Mo (TIMETAL 7-4) Annealed | Ti-8Al-1Mo-1V (TIMETAL 8-1-1) Annealed | Difference |
|---|---|---|---|
| Yield strength | 827 MPa | 827 MPa | 0% |
| Tensile strength | 896 MPa | 896 MPa | 0% |
| Elongation | 10 % | 10 % | 0% |
| Elastic modulus | 111,000 MPa | 121,000 MPa | +9% |
| Density | 4,480 kg/m³ | 4,370 kg/m³ | -2% |
| Thermal conductivity | 6.1 W/m·K | 5.98 W/m·K | -2% |
| Coefficient of thermal expansion | 0.00001 1/K | 0.000008 1/K | -13% |
| Reduction in area | 10 % | 20 % | +100% |
Difference is Ti-8Al-1Mo-1V (TIMETAL 8-1-1) Annealed relative to Ti-7Al-4Mo (TIMETAL 7-4) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-7Al-4Mo
- standard
- AMS 4919 / Mil-T-9047
- heat treatment
- Annealed
- grade
- Ti-8Al-1Mo-1V
- standard
- AMS 4915 / Mil-T-9047
- heat treatment
- Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators