Ti-5Al-2.5Sn Sheet Annealed vs Ti-5Al-2Sn-4Mo-2Zr-4Cr (TIMETAL 17) Solution Treated and Aged
Property comparison of Ti-5Al-2.5Sn Sheet Annealed and Ti-5Al-2Sn-4Mo-2Zr-4Cr (TIMETAL 17) Solution Treated and Aged, both titanium alloy.
| Property | Ti-5Al-2.5Sn Sheet Annealed | Ti-5Al-2Sn-4Mo-2Zr-4Cr (TIMETAL 17) Solution Treated and Aged | Difference |
|---|---|---|---|
| Yield strength | 779.1 MPa | 1,103 MPa | +42% |
| Tensile strength | 827.4 MPa | 1,172 MPa | +42% |
| Elongation | 10 % | 10 % | 0% |
| Elastic modulus | 106,869 MPa | 111,500 MPa | +4% |
| Density | 4,484 kg/m³ | 4,650 kg/m³ | +4% |
Difference is Ti-5Al-2Sn-4Mo-2Zr-4Cr (TIMETAL 17) Solution Treated and Aged relative to Ti-5Al-2.5Sn Sheet Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Ti-5Al-2.5Sn
- standard
- MIL-HDBK-5J
- heat treatment
- Annealed
- grade
- Ti-5Al-2Sn-4Mo-2Zr-4Cr
- standard
- AMS 4995
- heat treatment
- Solution Treated and Aged
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators