Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/Ti-3Al-2.5V-0.1Pd (ATI Grade 18) Annealed vs Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Annealed

Ti-3Al-2.5V-0.1Pd (ATI Grade 18) Annealed vs Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Annealed

Property comparison of Ti-3Al-2.5V-0.1Pd (ATI Grade 18) Annealed and Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Annealed, both titanium alloy.

Titanium Alloy4 compared properties
PropertyTi-3Al-2.5V-0.1Pd (ATI Grade 18) AnnealedTi-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) AnnealedDifference
Yield strength483 MPa758 MPa+57%
Tensile strength620 MPa827 MPa+33%
Elongation15 %10 %-33%
Density4,520 kg/m³4,820 kg/m³+7%

Difference is Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Annealed relative to Ti-3Al-2.5V-0.1Pd (ATI Grade 18) Annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Ti-3Al-2.5V-0.1Pd (ATI Grade 18) Annealed
grade
Ti-3Al-2.5V-0.1Pd
standard
ASTM B265 Grade 18
heat treatment
Annealed
Ti-3Al-8V-6Cr-4Mo-4Zr (ATI 38-644 / Beta C) Annealed
grade
Ti-3Al-8V-6Cr-4Mo-4Zr
standard
AMS 4957 / ASTM B348 Grade 19
heat treatment
Annealed (Solution Annealed)