Steel SAE 8660 vs Steel SAE 8740
Property comparison of Steel SAE 8660 and Steel SAE 8740, both carbon steel.
| Property | Steel SAE 8660 | Steel SAE 8740 | Difference |
|---|---|---|---|
| Yield strength | 1,551 MPa | 1,655 MPa | +7% |
| Tensile strength | 1,634 MPa | 1,999 MPa | +22% |
| Elongation | 13 % | 10 % | -23% |
| Elastic modulus | 207,000 MPa | 207,000 MPa | 0% |
| Shear modulus | 79,000 MPa | 79,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Brinell hardness | 460 HB | 578 HB | +26% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 467 J/kg·K | 462 J/kg·K | -1% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel SAE 8740 relative to Steel SAE 8660. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Steel SAE 8660
- standard
- ANSI
- heat treatment
- tempered at 800 F
Steel SAE 8740
- standard
- ANSI
- heat treatment
- tempered at 400 F
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators