Property comparison of Steel SAE 51414 and Steel SAE 51430, both carbon steel.

Carbon Steel12 compared properties
PropertySteel SAE 51414Steel SAE 51430Difference
Yield strength1,034 MPa310 MPa-70%
Tensile strength1,379 MPa517 MPa-63%
Elongation15 %30 %+100%
Elastic modulus200,000 MPa200,000 MPa0%
Shear modulus769,000 MPa769,000 MPa0%
Poisson ratio0.30.30%
Density8,030 kg/m³8,030 kg/m³0%
Brinell hardness415 HB155 HB-63%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat463 J/kg·K463 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel SAE 51430 relative to Steel SAE 51414. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel SAE 51414
standard
ANSI
heat treatment
tempered at 400 F
Steel SAE 51430
standard
ANSI
heat treatment
annealed

What else is in Engineering Database

Related comparisons

View each material