| Property | Steel SAE 30314 | Steel SAE 30317 | Difference |
|---|---|---|---|
| Yield strength | 345 MPa | 276 MPa | -20% |
| Tensile strength | 689 MPa | 621 MPa | -10% |
| Elongation | 45 % | 50 % | +11% |
| Elastic modulus | 193,000 MPa | 193,000 MPa | 0% |
| Shear modulus | 743,000 MPa | 743,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 8,030 kg/m³ | 8,030 kg/m³ | 0% |
| Brinell hardness | 170 HB | 160 HB | -6% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel SAE 30317 relative to Steel SAE 30314. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Steel SAE 30314
- standard
- ANSI
- heat treatment
- annealed
Steel SAE 30317
- standard
- ANSI
- heat treatment
- annealed
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators