Steel SAE 1050 vs Steel SAE 1060

Property comparison of Steel SAE 1050 and Steel SAE 1060, both carbon steel.

Carbon Steel12 compared properties
PropertySteel SAE 1050Steel SAE 1060Difference
Yield strength414 MPa483 MPa+17%
Tensile strength724 MPa814 MPa+12%
Elongation20 %17 %-15%
Elastic modulus207,000 MPa207,000 MPa0%
Shear modulus79,000 MPa79,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Brinell hardness229 HB241 HB+5%
Thermal conductivity54 W/m·K51.9 W/m·K-4%
Specific heat465 J/kg·K467 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel SAE 1060 relative to Steel SAE 1050. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel SAE 1050
standard
ANSI
heat treatment
as-rolled
Steel SAE 1060
standard
ANSI
heat treatment
as-rolled

What else is in Engineering Database

Related comparisons

View each material