Steel A11 GOST 1414-75 vs Steel A12 GOST 1414-75

Property comparison of Steel A11 GOST 1414-75 and Steel A12 GOST 1414-75, both carbon steel.

Carbon Steel12 compared properties
PropertySteel A11 GOST 1414-75Steel A12 GOST 1414-75Difference
Yield strength390 MPa390 MPa0%
Tensile strength490 MPa460 MPa-6%
Elongation10 %7 %-30%
Elastic modulus216,000 MPa216,000 MPa0%
Shear modulus83,000 MPa83,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Brinell hardness207 HB217 HB+5%
Thermal conductivity68.8 W/m·K68.4 W/m·K-1%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel A12 GOST 1414-75 relative to Steel A11 GOST 1414-75. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.