Steel 55 GOST 1577-93 vs Steel 60 GOST 1050-88
Property comparison of Steel 55 GOST 1577-93 and Steel 60 GOST 1050-88, both carbon steel.
| Property | Steel 55 GOST 1577-93 | Steel 60 GOST 1050-88 | Difference |
|---|---|---|---|
| Yield strength | 430 MPa | 450 MPa | +5% |
| Tensile strength | 775 MPa | 825 MPa | +6% |
| Elongation | 15 % | 14 % | -7% |
| Elastic modulus | 206,000 MPa | 204,000 MPa | -1% |
| Shear modulus | 80,000 MPa | 79,000 MPa | -1% |
| Poisson ratio | 0.29 | 0.29 | 0% |
| Density | 7,860 kg/m³ | 7,810 kg/m³ | -1% |
| Thermal conductivity | 52.9 W/m·K | 51.9 W/m·K | -2% |
| Specific heat | 466 J/kg·K | 467 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel 60 GOST 1050-88 relative to Steel 55 GOST 1577-93. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- GOST
- heat treatment
- Quenched and tempered
- standard
- GOST
- heat treatment
- Quenched and tempered
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators