Steel 32Ch06L GOST 977-88 vs Steel 35 GOST 1050-88
Property comparison of Steel 32Ch06L GOST 977-88 and Steel 35 GOST 1050-88, both carbon steel.
| Property | Steel 32Ch06L GOST 977-88 | Steel 35 GOST 1050-88 | Difference |
|---|---|---|---|
| Yield strength | 491 MPa | 310 MPa | -37% |
| Tensile strength | 638 MPa | 470 MPa | -26% |
| Elongation | 12 % | 15 % | +25% |
| Elastic modulus | 205,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 79,000 MPa | 79,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,850 kg/m³ | 7,826 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 59.7 W/m·K | +15% |
| Specific heat | 460 J/kg·K | 461 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel 35 GOST 1050-88 relative to Steel 32Ch06L GOST 977-88. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- GOST
- heat treatment
- Quenched and tempered
- standard
- GOST
- heat treatment
- Annealing or high tempering
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators