| Property | Steel 30 GOST 1577-93 | Steel 30Ch GOST 4543-71 | Difference |
|---|---|---|---|
| Yield strength | 280 MPa | 685 MPa | +145% |
| Tensile strength | 540 MPa | 880 MPa | +63% |
| Elongation | 23 % | 12 % | -48% |
| Elastic modulus | 206,000 MPa | 208,000 MPa | +1% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.29 | 0.3 | +3% |
| Density | 7,860 kg/m³ | 7,820 kg/m³ | -1% |
| Brinell hardness | 179 HB | 187 HB | +4% |
| Thermal conductivity | 61.6 W/m·K | 51.9 W/m·K | -16% |
| Specific heat | 460 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is Steel 30Ch GOST 4543-71 relative to Steel 30 GOST 1577-93. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- standard
- GOST
- heat treatment
- normalized
- standard
- GOST
- heat treatment
- —
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators