Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/Steel 12Ch7G3SL GOST 977-88 vs Steel 12Ch8VF GOST 20072-74

Steel 12Ch7G3SL GOST 977-88 vs Steel 12Ch8VF GOST 20072-74

Property comparison of Steel 12Ch7G3SL GOST 977-88 and Steel 12Ch8VF GOST 20072-74, both carbon steel.

Carbon Steel11 compared properties
PropertySteel 12Ch7G3SL GOST 977-88Steel 12Ch8VF GOST 20072-74Difference
Yield strength1,079 MPa165 MPa-85%
Tensile strength1,324 MPa390 MPa-71%
Elongation9 %22 %+144%
Elastic modulus200,000 MPa200,000 MPa0%
Shear modulus77,000 MPa77,000 MPa0%
Poisson ratio0.30.30%
Density7,820 kg/m³7,850 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 12Ch8VF GOST 20072-74 relative to Steel 12Ch7G3SL GOST 977-88. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 12Ch7G3SL GOST 977-88
standard
GOST
heat treatment
Quenched and tempered
Steel 12Ch8VF GOST 20072-74
standard
GOST
heat treatment

What else is in Engineering Database