Property comparison of Steel 10 GOST 1050-88 and Steel 10Ch11N23T3MR GOST 5949-75, both carbon steel.

Carbon Steel11 compared properties
PropertySteel 10 GOST 1050-88Steel 10Ch11N23T3MR GOST 5949-75Difference
Yield strength205 MPa685 MPa+234%
Tensile strength330 MPa980 MPa+197%
Elongation31 %10 %-68%
Elastic modulus206,000 MPa200,000 MPa-3%
Shear modulus79,000 MPa77,000 MPa-3%
Poisson ratio0.30.30%
Density7,856 kg/m³8,120 kg/m³+3%
Thermal conductivity69.2 W/m·K51.9 W/m·K-25%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 10Ch11N23T3MR GOST 5949-75 relative to Steel 10 GOST 1050-88. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 10 GOST 1050-88
standard
GOST
heat treatment
normalized
Steel 10Ch11N23T3MR GOST 5949-75
standard
GOST
heat treatment

What else is in Engineering Database

Related comparisons

View each material