Stainless Steel12 compared properties
PropertySAE 321 Stainless Steel (Annealed sheet)SAE 330 Stainless Steel (Annealed bar)Difference
Yield strength240 MPa290 MPa+21%
Tensile strength620 MPa585 MPa-6%
Elongation45 %45 %0%
Elastic modulus193,000 MPa193,000 MPa0%
Shear modulus74,231 MPa74,231 MPa0%
Poisson ratio0.30.30%
Density7,850 kg/m³7,850 kg/m³0%
Brinell hardness147 HB147 HB0%
Thermal conductivity15.1 W/m·K15.1 W/m·K0%
Specific heat460 J/kg·K500 J/kg·K+9%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,400 °C1,400 °C0%

Difference is SAE 330 Stainless Steel (Annealed bar) relative to SAE 321 Stainless Steel (Annealed sheet). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

SAE 321 Stainless Steel (Annealed sheet)
grade
321
standard
SAE
heat treatment
Annealed sheet
SAE 330 Stainless Steel (Annealed bar)
grade
330
standard
SAE
heat treatment
Annealed bar

About 300-series stainless steels

Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.

What else is in Engineering Database

Related comparisons

View each material