Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Stainless Steel/SAE 303 Stainless Steel (Annealed bar) vs SAE 304 Stainless Steel (Annealed bar)

SAE 303 Stainless Steel (Annealed bar) vs SAE 304 Stainless Steel (Annealed bar)

Property comparison of SAE 303 Stainless Steel (Annealed bar) and SAE 304 Stainless Steel (Annealed bar), both stainless steel.

Stainless Steel13 compared properties
PropertySAE 303 Stainless Steel (Annealed bar)SAE 304 Stainless Steel (Annealed bar)Difference
Yield strength240 MPa235 MPa-2%
Tensile strength620 MPa585 MPa-6%
Elongation50 %60 %+20%
Elastic modulus193,000 MPa193,000 MPa0%
Shear modulus74,231 MPa74,231 MPa0%
Poisson ratio0.30.30%
Density7,850 kg/m³7,850 kg/m³0%
Brinell hardness160 HB149 HB-7%
Thermal conductivity15.1 W/m·K15.1 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,400 °C1,400 °C0%
Reduction in area55 %70 %+27%

Difference is SAE 304 Stainless Steel (Annealed bar) relative to SAE 303 Stainless Steel (Annealed bar). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

SAE 303 Stainless Steel (Annealed bar)
grade
303
standard
SAE
heat treatment
Annealed bar
SAE 304 Stainless Steel (Annealed bar)
grade
304
standard
SAE
heat treatment
Annealed bar

About 300-series stainless steels

Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.

What else is in Engineering Database

Related comparisons

View each material