SAE 201 Stainless Steel (50% hard) vs SAE 202 Stainless Steel (50% hard sheet)

Property comparison of SAE 201 Stainless Steel (50% hard) and SAE 202 Stainless Steel (50% hard sheet), both stainless steel.

Stainless Steel11 compared properties
PropertySAE 201 Stainless Steel (50% hard)SAE 202 Stainless Steel (50% hard sheet)Difference
Yield strength760 MPa760 MPa0%
Tensile strength1,035 MPa1,030 MPa0%
Elongation12 %10 %-17%
Elastic modulus193,000 MPa193,000 MPa0%
Shear modulus74,231 MPa74,231 MPa0%
Poisson ratio0.30.30%
Density7,850 kg/m³7,850 kg/m³0%
Thermal conductivity15.1 W/m·K15.1 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000016 1/K0.000016 1/K0%
Melting point1,400 °C1,400 °C0%

Difference is SAE 202 Stainless Steel (50% hard sheet) relative to SAE 201 Stainless Steel (50% hard). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

SAE 201 Stainless Steel (50% hard)
grade
201
standard
SAE
heat treatment
50% hard
SAE 202 Stainless Steel (50% hard sheet)
grade
202
standard
SAE
heat treatment
50% hard sheet

About 200-series stainless steels

200-series grades substitute manganese and nitrogen for some of the nickel found in the 300-series. They have similar corrosion behavior to 304 in mild environments at lower alloy cost but reduced performance in chloride and pitting service. Cold work hardens them more aggressively than the 300-series.