SAE 1086 Carbon Steel (Hot rolled) vs SAE 1090 Carbon Steel (Hot rolled)
Property comparison of SAE 1086 Carbon Steel (Hot rolled) and SAE 1090 Carbon Steel (Hot rolled), both carbon steel.
| Property | SAE 1086 Carbon Steel (Hot rolled) | SAE 1090 Carbon Steel (Hot rolled) | Difference |
|---|---|---|---|
| Yield strength | 425 MPa | 460 MPa | +8% |
| Tensile strength | 770 MPa | 840 MPa | +9% |
| Elongation | 10 % | 10 % | 0% |
| Elastic modulus | 200,000 MPa | 200,000 MPa | 0% |
| Shear modulus | 76,923 MPa | 76,923 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,850 kg/m³ | 7,850 kg/m³ | 0% |
| Brinell hardness | 229 HB | 248 HB | +8% |
| Thermal conductivity | 46.1 W/m·K | 45.2 W/m·K | -2% |
| Specific heat | 471 J/kg·K | 471 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
| Reduction in area | 25 % | 25 % | 0% |
Difference is SAE 1090 Carbon Steel (Hot rolled) relative to SAE 1086 Carbon Steel (Hot rolled). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- 1086
- standard
- SAE
- heat treatment
- Hot rolled
- grade
- 1090
- standard
- SAE
- heat treatment
- Hot rolled
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators