SAE 1043 Carbon Steel (Normalized, Cold drawn) vs SAE 1044 Carbon Steel (Hot rolled)

Property comparison of SAE 1043 Carbon Steel (Normalized, Cold drawn) and SAE 1044 Carbon Steel (Hot rolled), both carbon steel.

Carbon Steel13 compared properties
PropertySAE 1043 Carbon Steel (Normalized, Cold drawn)SAE 1044 Carbon Steel (Hot rolled)Difference
Yield strength515 MPa305 MPa-41%
Tensile strength600 MPa550 MPa-8%
Elongation12 %16 %+33%
Elastic modulus200,000 MPa200,000 MPa0%
Shear modulus76,923 MPa76,923 MPa0%
Poisson ratio0.30.30%
Density7,850 kg/m³7,850 kg/m³0%
Brinell hardness179 HB163 HB-9%
Thermal conductivity56.7 W/m·K56.3 W/m·K-1%
Specific heat463 J/kg·K463 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%
Reduction in area45 %40 %-11%

Difference is SAE 1044 Carbon Steel (Hot rolled) relative to SAE 1043 Carbon Steel (Normalized, Cold drawn). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

SAE 1043 Carbon Steel (Normalized, Cold drawn)
grade
1043
standard
SAE
heat treatment
Normalized, Cold drawn
SAE 1044 Carbon Steel (Hot rolled)
grade
1044
standard
SAE
heat treatment
Hot rolled

What else is in Engineering Database

Related comparisons

View each material