Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Copper Alloy/Red brass C83300 vs Red brass C83400

Red brass C83300 vs Red brass C83400

Property comparison of Red brass C83300 and Red brass C83400, both copper alloy.

Copper Alloy11 compared properties
PropertyRed brass C83300Red brass C83400Difference
Yield strength69 MPa69 MPa0%
Tensile strength221 MPa241 MPa+9%
Elongation35 %30 %-14%
Elastic modulus100,000 MPa100,000 MPa0%
Shear modulus37,000 MPa37,000 MPa0%
Poisson ratio0.340.340%
Density8,720 kg/m³8,720 kg/m³0%
Thermal conductivity72 W/m·K72 W/m·K0%
Specific heat385 J/kg·K385 J/kg·K0%
Coefficient of thermal expansion0.000018 1/K0.000018 1/K0%
Melting point977 °C977 °C0%

Difference is Red brass C83400 relative to Red brass C83300. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Red brass C83300
standard
ANSI
Red brass C83400
standard
ANSI

About brass copper alloys

Brass is the copper-zinc alloy family. C26000 (cartridge brass, 70/30) is the standard for deep drawing, ammunition cases, and decorative work. Higher-zinc brasses such as C36000 (free-cutting) are the standard for screw-machine work. Lead-free brass is increasingly required for potable-water service.