PropertyPOM Homopolymer (Acetal/Delrin)PPO/PS Blend GF20 (Noryl GFN2)Difference
Tensile strength69 MPa117 MPa+70%
Elongation40 %3 %-93%
Poisson ratio0.350.38+9%
Density1,420 kg/m³1,270 kg/m³-11%
Thermal conductivity0.37 W/m·K0.19 W/m·K-49%
Specific heat1,460 J/kg·K1,300 J/kg·K-11%
Coefficient of thermal expansion0.000106 1/K0.000035 1/K-67%

Difference is PPO/PS Blend GF20 (Noryl GFN2) relative to POM Homopolymer (Acetal/Delrin). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

POM Homopolymer (Acetal/Delrin)
standard
ASTM
PPO/PS Blend GF20 (Noryl GFN2)
standard
ASTM

What else is in Engineering Database

Related comparisons

View each material