Nodular cast iron 80 GOST7293-85 vs Nodular cast iron

Property comparison of Nodular cast iron 80 GOST7293-85 and Nodular cast iron, both cast iron.

Cast Iron10 compared properties
PropertyNodular cast iron 80 GOST7293-85Nodular cast ironDifference
Yield strength480 MPa420 MPa-13%
Tensile strength800 MPa700 MPa-13%
Elastic modulus180,000 MPa169,000 MPa-6%
Shear modulus75,000 MPa70,000 MPa-7%
Poisson ratio0.20.20%
Density7,160 kg/m³7,160 kg/m³0%
Thermal conductivity36 W/m·K36 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000011 1/K0.000011 1/K0%
Melting point1,150 °C1,150 °C0%

Difference is Nodular cast iron relative to Nodular cast iron 80 GOST7293-85. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Nodular cast iron 80 GOST7293-85
standard
GOST
Nodular cast iron
standard
BS

About ductile (nodular) cast iron

Ductile iron, also called nodular or spheroidal graphite iron, has graphite in spherical form rather than flakes. The microstructure gives it tensile strength and ductility much closer to steel than gray iron, while retaining cast-iron's castability. It is the standard for water and sewer pipe, pump housings, and crankshafts. ASTM A536 grades (60-40-18, 80-55-06, etc.) report tensile, yield, and elongation.