Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/NiTiNb (Shape Memory, As > 30°C, cryogenic Ms) vs Ti 15V 3CR 3SN 3AL

NiTiNb (Shape Memory, As > 30°C, cryogenic Ms) vs Ti 15V 3CR 3SN 3AL

Property comparison of NiTiNb (Shape Memory, As > 30°C, cryogenic Ms) and Ti 15V 3CR 3SN 3AL, both titanium alloy.

Titanium Alloy5 compared properties
PropertyNiTiNb (Shape Memory, As > 30°C, cryogenic Ms)Ti 15V 3CR 3SN 3ALDifference
Yield strength414 MPa1,172 MPa+183%
Tensile strength648 MPa1,241 MPa+92%
Elongation15 %5 %-67%
Density6,450 kg/m³4,780 kg/m³-26%
Melting point1,310 °C760 °C-42%

Difference is Ti 15V 3CR 3SN 3AL relative to NiTiNb (Shape Memory, As > 30°C, cryogenic Ms). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NiTiNb (Shape Memory, As > 30°C, cryogenic Ms)
grade
Ni-46-50Ti-8-15Nb
standard
ATI Proprietary
heat treatment
Solution Annealed
Ti 15V 3CR 3SN 3AL
grade
Ti-15V-3Cr-3Sn-3Al
standard
AMS 4914
heat treatment
Solution Treated and Aged (16hr/900°F/482°C)

What else is in Engineering Database

Related comparisons

View each material