Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Titanium Alloy/NiTi SEA 1 (Superelastic, Af -30°C to 0°C) vs CP Ti Grade 16 (Ti-0.05Pd) Annealed

NiTi SEA 1 (Superelastic, Af -30°C to 0°C) vs CP Ti Grade 16 (Ti-0.05Pd) Annealed

Property comparison of NiTi SEA 1 (Superelastic, Af -30°C to 0°C) and CP Ti Grade 16 (Ti-0.05Pd) Annealed, both titanium alloy.

Titanium Alloy3 compared properties
PropertyNiTi SEA 1 (Superelastic, Af -30°C to 0°C)CP Ti Grade 16 (Ti-0.05Pd) AnnealedDifference
Tensile strength1,070 MPa345 MPa-68%
Elongation10 %20 %+100%
Density6,450 kg/m³4,520 kg/m³-30%

Difference is CP Ti Grade 16 (Ti-0.05Pd) Annealed relative to NiTi SEA 1 (Superelastic, Af -30°C to 0°C). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NiTi SEA 1 (Superelastic, Af -30°C to 0°C)
grade
Ni-55Ti (SEA 1)
standard
ASTM F2063
heat treatment
Solution Annealed
CP Ti Grade 16 (Ti-0.05Pd) Annealed
grade
CP Ti Grade 16
standard
ASTM B265 Grade 16
heat treatment
Annealed

What else is in Engineering Database

Related comparisons

View each material