NF Z8CA7 vs SAE 12L14 Carbon Steel (Cold drawn)

Property comparison of NF Z8CA7 and SAE 12L14 Carbon Steel (Cold drawn), both carbon steel.

Carbon Steel11 compared properties
PropertyNF Z8CA7SAE 12L14 Carbon Steel (Cold drawn)Difference
Yield strength240 MPa415 MPa+73%
Tensile strength440 MPa540 MPa+23%
Elongation24 %10 %-58%
Elastic modulus206,000 MPa200,000 MPa-3%
Shear modulus80,000 MPa76,923 MPa-4%
Poisson ratio0.30.30%
Density7,860 kg/m³7,850 kg/m³0%
Thermal conductivity51.9 W/m·K67.3 W/m·K+30%
Specific heat460 J/kg·K456 J/kg·K-1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is SAE 12L14 Carbon Steel (Cold drawn) relative to NF Z8CA7. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF Z8CA7
standard
NF
grade
heat treatment
SAE 12L14 Carbon Steel (Cold drawn)
standard
SAE
grade
12L14
heat treatment
Cold drawn

What else is in Engineering Database

Related comparisons

View each material