Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/NF Z6CN1809 vs NF Z6CNDT1712

NF Z6CN1809 vs NF Z6CNDT1712

Property comparison of NF Z6CN1809 and NF Z6CNDT1712, both carbon steel.

Carbon Steel11 compared properties
PropertyNF Z6CN1809NF Z6CNDT1712Difference
Yield strength195 MPa216 MPa+11%
Tensile strength510 MPa490 MPa-4%
Elongation45 %40 %-11%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF Z6CNDT1712 relative to NF Z6CN1809. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF Z6CN1809
standard
NF
NF Z6CNDT1712
standard
NF

What else is in Engineering Database

Related comparisons

View each material