Property comparison of NF XC18 and NF XC32, both carbon steel.

Carbon Steel11 compared properties
PropertyNF XC18NF XC32Difference
Yield strength270 MPa365 MPa+35%
Tensile strength440 MPa570 MPa+30%
Elongation21 %18 %-14%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.2 W/m·K60.8 W/m·K-8%
Specific heat457 J/kg·K460 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF XC32 relative to NF XC18. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF XC18
standard
NF
NF XC32
standard
NF

What else is in Engineering Database

Related comparisons

View each material