NF 38C4 vs NF 42CD4TS
Property comparison of NF 38C4 and NF 42CD4TS, both carbon steel.
| Property | NF 38C4 | NF 42CD4TS | Difference |
|---|---|---|---|
| Yield strength | 620 MPa | 815 MPa | +31% |
| Tensile strength | 830 MPa | 980 MPa | +18% |
| Elongation | 13 % | 11 % | -15% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 58.6 W/m·K | 51.9 W/m·K | -11% |
| Specific heat | 462 J/kg·K | 463 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is NF 42CD4TS relative to NF 38C4. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
NF 38C4
- standard
- NF
- heat treatment
- —
NF 42CD4TS
- standard
- NF
- heat treatment
- face hardened
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators