Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
NF 30CND8 vs NF 34CD4
Property comparison of NF 30CND8 and NF 34CD4, both carbon steel.
| Property | NF 30CND8 | NF 34CD4 | Difference |
|---|---|---|---|
| Yield strength | 850 MPa | 700 MPa | -18% |
| Tensile strength | 1,030 MPa | 880 MPa | -15% |
| Elongation | 12 % | 12 % | 0% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 461 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is NF 34CD4 relative to NF 30CND8. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
NF 30CND8
- standard
- NF
- heat treatment
- heat treated
NF 34CD4
- standard
- NF
- heat treatment
- —
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators