Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/NF 18NCD6 vs NF 30CD12

NF 18NCD6 vs NF 30CD12

Property comparison of NF 18NCD6 and NF 30CD12, both carbon steel.

Carbon Steel11 compared properties
PropertyNF 18NCD6NF 30CD12Difference
Yield strength850 MPa810 MPa-5%
Tensile strength1,200 MPa1,030 MPa-14%
Elongation8 %10 %+25%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat457 J/kg·K460 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF 30CD12 relative to NF 18NCD6. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

NF 18NCD6
standard
NF
heat treatment
case-hardened
NF 30CD12
standard
NF
heat treatment
heat treated