Meteorite Iron Taenite (Fe-30Ni) vs Pure Chromium (Cr 99.9%+)
Property comparison of Meteorite Iron Taenite (Fe-30Ni) and Pure Chromium (Cr 99.9%+), both pure metal.
| Property | Meteorite Iron Taenite (Fe-30Ni) | Pure Chromium (Cr 99.9%+) | Difference |
|---|---|---|---|
| Yield strength | 400 MPa | 131 MPa | -67% |
| Tensile strength | 700 MPa | 550 MPa | -21% |
| Elongation | 8 % | 0 % | -100% |
| Elastic modulus | 185,000 MPa | 279,000 MPa | +51% |
| Density | 8,000 kg/m³ | 7,190 kg/m³ | -10% |
| Thermal conductivity | 18 W/m·K | 67 W/m·K | +272% |
| Coefficient of thermal expansion | 0.000013 1/K | 0.000006 1/K | -52% |
| Melting point | 1,450 °C | 1,875 °C | +29% |
Difference is Pure Chromium (Cr 99.9%+) relative to Meteorite Iron Taenite (Fe-30Ni). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- Fe-30Ni gamma phase (taenite)
- standard
- Buchwald "Handbook of Iron Meteorites" (1975) / Smithells Metals Reference Book
- heat treatment
- meteoritic (very slow cooled)
- grade
- electrolytic chromium
- standard
- ESPI Metals chromium technical data / AZoM ArticleID 594
- heat treatment
- —
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators