PropertyMeteorite Iron Kamacite (Fe-7Ni)Pure Nickel (Ni 99.6+ Nickel 200)Difference
Yield strength250 MPa148 MPa-41%
Tensile strength400 MPa462 MPa+16%
Elongation15 %47 %+213%
Elastic modulus195,000 MPa204,000 MPa+5%
Density7,900 kg/m³8,900 kg/m³+13%
Thermal conductivity40 W/m·K91 W/m·K+127%
Coefficient of thermal expansion0.000012 1/K0.000013 1/K+11%
Melting point1,510 °C1,455 °C-4%

Difference is Pure Nickel (Ni 99.6+ Nickel 200) relative to Meteorite Iron Kamacite (Fe-7Ni). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Meteorite Iron Kamacite (Fe-7Ni)
grade
Fe-7Ni alpha phase (kamacite)
standard
Buchwald "Handbook of Iron Meteorites" (1975) / Smithells Metals Reference Book
heat treatment
meteoritic (very slow cooled)
Pure Nickel (Ni 99.6+ Nickel 200)
grade
Nickel 200 / N02200
standard
Special Metals Nickel 200 technical bulletin / NIST elastic properties
heat treatment
annealed