PropertyLeaded Tin Bronze C92600Leaded Tin Bronze C92900Difference
Yield strength138 MPa179 MPa+30%
Tensile strength303 MPa324 MPa+7%
Elongation30 %20 %-33%
Elastic modulus120,000 MPa120,000 MPa0%
Shear modulus45,000 MPa45,000 MPa0%
Poisson ratio0.310.310%
Density8,800 kg/m³8,800 kg/m³0%
Thermal conductivity52 W/m·K52 W/m·K0%
Specific heat377 J/kg·K377 J/kg·K0%
Coefficient of thermal expansion0.000018 1/K0.000018 1/K0%
Melting point960 °C960 °C0%

Difference is Leaded Tin Bronze C92900 relative to Leaded Tin Bronze C92600. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Leaded Tin Bronze C92600
standard
ANSI
Leaded Tin Bronze C92900
standard
ANSI