PropertyJIS STKM13BJIS STKM16CDifference
Yield strength305 MPa460 MPa+51%
Tensile strength440 MPa620 MPa+41%
Elongation20 %12 %-40%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity65.4 W/m·K65.4 W/m·K0%
Specific heat457 J/kg·K457 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is JIS STKM16C relative to JIS STKM13B. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

JIS STKM13B
standard
JIS
JIS STKM16C
standard
JIS

What else is in Engineering Database

Related comparisons

View each material