Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/Inconel 706 vs Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) aged

Inconel 706 vs Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) aged

Property comparison of Inconel 706 and Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) aged, both nickel alloy.

Nickel Alloy8 compared properties
PropertyInconel 706Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) agedDifference
Yield strength383 MPa818 MPa+114%
Tensile strength757 MPa1,209 MPa+60%
Elongation47 %36 %-23%
Elastic modulus210,000 MPa221,000 MPa+5%
Density8,050 kg/m³8,050 kg/m³0%
Thermal conductivity12.5 W/m·K10.2 W/m·K-18%
Coefficient of thermal expansion0.000014 1/K0.000012 1/K-8%
Melting point1,360 °C1,362 °C0%

Difference is Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) aged relative to Inconel 706. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Inconel 706
grade
N09706
standard
Special Metals Corp. tech bulletin INCONEL alloy 706; AZoM ArticleID 7697
heat treatment
annealed
Inconel 740 (Ni-25Cr-20Co-2Nb-2Ti) aged
grade
N07740
standard
Special Metals Corp. tech bulletin INCONEL alloy 740; AZoM ArticleID 9446
heat treatment
precipitation hardened

About Inconel nickel-chromium superalloys

Inconel is a family of nickel-chromium-iron superalloys. They keep strength at temperatures where steels and most stainless grades have failed and resist oxidation and hot corrosion. Inconel 718 is the most widely used grade for aerospace turbine disks and high-temperature fasteners; Inconel 625 is the choice when chloride and reducing-acid corrosion both matter.

What else is in Engineering Database

Related comparisons

View each material