Haynes HR 120 vs N 155
Property comparison of Haynes HR 120 and N 155, both nickel alloy.
| Property | Haynes HR 120 | N 155 | Difference |
|---|---|---|---|
| Yield strength | 275.8 MPa | 337.85 MPa | +23% |
| Tensile strength | 620.55 MPa | 689.5 MPa | +11% |
| Elongation | 30 % | 40 % | +33% |
| Density | 8,968 kg/m³ | 8,304 kg/m³ | -7% |
Difference is N 155 relative to Haynes HR 120. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Haynes HR 120
- grade
- HAYNES HR-120
- standard
- MIL-HDBK-5J
- heat treatment
- Annealed
N 155
- grade
- N-155
- standard
- MIL-HDBK-5J
- heat treatment
- Solution Treated
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators