Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
EN X8Ni9 vs NF 13MF4
Property comparison of EN X8Ni9 and NF 13MF4, both carbon steel.
| Property | EN X8Ni9 | NF 13MF4 | Difference |
|---|---|---|---|
| Yield strength | 585 MPa | 240 MPa | -59% |
| Tensile strength | 680 MPa | 360 MPa | -47% |
| Elongation | 18 % | 26 % | +44% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 455 J/kg·K | -1% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is NF 13MF4 relative to EN X8Ni9. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
EN X8Ni9
- standard
- ISO
NF 13MF4
- standard
- NF
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators