PropertyEN X6CrNiMoTi17-12-2NF 15CD405Difference
Yield strength200 MPa295 MPa+48%
Tensile strength500 MPa450 MPa-10%
Elongation40 %20 %-50%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat460 J/kg·K456 J/kg·K-1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is NF 15CD405 relative to EN X6CrNiMoTi17-12-2. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN X6CrNiMoTi17-12-2
standard
ISO
NF 15CD405
standard
NF

What else is in Engineering Database

Related comparisons

View each material