Home/Compare/Carbon Steel/EN X6Cr13 vs EN X6Cr17

EN X6Cr13 vs EN X6Cr17

Property comparison of EN X6Cr13 and EN X6Cr17, both carbon steel.

Carbon Steel11 compared properties
PropertyEN X6Cr13EN X6Cr17Difference
Yield strength230 MPa240 MPa+4%
Tensile strength400 MPa400 MPa0%
Elongation20 %20 %0%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN X6Cr17 relative to EN X6Cr13. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.