EN X2CrNiMoN22-5-3 vs EN X30Cr13
Property comparison of EN X2CrNiMoN22-5-3 and EN X30Cr13, both carbon steel.
| Property | EN X2CrNiMoN22-5-3 | EN X30Cr13 | Difference |
|---|---|---|---|
| Yield strength | 450 MPa | 650 MPa | +44% |
| Tensile strength | 650 MPa | 850 MPa | +31% |
| Elongation | 25 % | 10 % | -60% |
| Elastic modulus | 206,000 MPa | 206,000 MPa | 0% |
| Shear modulus | 80,000 MPa | 80,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 7,860 kg/m³ | 7,860 kg/m³ | 0% |
| Thermal conductivity | 51.9 W/m·K | 51.9 W/m·K | 0% |
| Specific heat | 460 J/kg·K | 460 J/kg·K | 0% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | 0% |
| Melting point | 1,480 °C | 1,480 °C | 0% |
Difference is EN X30Cr13 relative to EN X2CrNiMoN22-5-3. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
EN X2CrNiMoN22-5-3
- standard
- ISO
EN X30Cr13
- standard
- ISO
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators