PropertyEN X17CrNi16-2EN X20Cr13Difference
Yield strength600 MPa500 MPa-17%
Tensile strength800 MPa700 MPa-13%
Elongation14 %13 %-7%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN X20Cr13 relative to EN X17CrNi16-2. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN X17CrNi16-2
standard
ISO
EN X20Cr13
standard
ISO

What else is in Engineering Database

Related comparisons

View each material