Home/Compare/Carbon Steel/EN C60 vs EN E355

EN C60 vs EN E355

Property comparison of EN C60 and EN E355, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C60EN E355Difference
Yield strength520 MPa325 MPa-38%
Tensile strength800 MPa570 MPa-29%
Elongation13 %16 %+23%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K65.4 W/m·K+26%
Specific heat467 J/kg·K457 J/kg·K-2%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN E355 relative to EN C60. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C60
standard
ISO
heat treatment
heat treated
EN E355
standard
ISO
heat treatment

What else is in Engineering Database

Related comparisons

View each material