Property comparison of EN C30 and EN C55, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C30EN C55Difference
Yield strength350 MPa490 MPa+40%
Tensile strength550 MPa750 MPa+36%
Elongation20 %14 %-30%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity61.6 W/m·K52.9 W/m·K-14%
Specific heat460 J/kg·K466 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C55 relative to EN C30. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C30
standard
ISO
heat treatment
EN C55
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material