Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/EN C15E vs EN C25

EN C15E vs EN C25

Property comparison of EN C15E and EN C25, both carbon steel.

Carbon Steel11 compared properties
PropertyEN C15EEN C25Difference
Yield strength340 MPa320 MPa-6%
Tensile strength440 MPa500 MPa+14%
Elongation11 %21 %+91%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity67.3 W/m·K63.5 W/m·K-6%
Specific heat456 J/kg·K458 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C25 relative to EN C15E. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C15E
standard
ISO
EN C25
standard
ISO

What else is in Engineering Database