PropertyEN C10EEN C22Difference
Yield strength300 MPa290 MPa-3%
Tensile strength420 MPa470 MPa+12%
Elongation16 %22 %+38%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity69.2 W/m·K64.6 W/m·K-7%
Specific heat455 J/kg·K458 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN C22 relative to EN C10E. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN C10E
standard
ISO
EN C22
standard
ISO

What else is in Engineering Database

Related comparisons

View each material