Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/EN 35S20 vs EN 37Cr4

EN 35S20 vs EN 37Cr4

Property comparison of EN 35S20 and EN 37Cr4, both carbon steel.

Carbon Steel11 compared properties
PropertyEN 35S20EN 37Cr4Difference
Yield strength380 MPa630 MPa+66%
Tensile strength600 MPa850 MPa+42%
Elongation16 %13 %-19%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity59.7 W/m·K51.9 W/m·K-13%
Specific heat461 J/kg·K462 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 37Cr4 relative to EN 35S20. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 35S20
standard
ISO
heat treatment
EN 37Cr4
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material