Property comparison of EN 16NiCr4 and EN 25CrMo4, both carbon steel.

Carbon Steel11 compared properties
PropertyEN 16NiCr4EN 25CrMo4Difference
Yield strength590 MPa600 MPa+2%
Tensile strength835 MPa800 MPa-4%
Elongation12 %14 %+17%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat456 J/kg·K458 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is EN 25CrMo4 relative to EN 16NiCr4. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

EN 16NiCr4
standard
ISO
heat treatment
case-hardened
EN 25CrMo4
standard
ISO
heat treatment
heat treated

What else is in Engineering Database

Related comparisons

View each material