PropertyDIN X6Cr17DIN X6CrAl13Difference
Yield strength270 MPa250 MPa-7%
Tensile strength450 MPa400 MPa-11%
Elongation20 %20 %0%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat460 J/kg·K460 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN X6CrAl13 relative to DIN X6Cr17. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN X6Cr17
standard
DIN
DIN X6CrAl13
standard
DIN

What else is in Engineering Database

Related comparisons

View each material