PropertyDIN USt34-2DIN X20Cr13Difference
Yield strength195 MPa450 MPa+131%
Tensile strength330 MPa650 MPa+97%
Elongation28 %14 %-50%
Elastic modulus206,000 MPa206,000 MPa0%
Shear modulus80,000 MPa80,000 MPa0%
Poisson ratio0.30.30%
Density7,860 kg/m³7,860 kg/m³0%
Thermal conductivity66.5 W/m·K51.9 W/m·K-22%
Specific heat456 J/kg·K460 J/kg·K+1%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is DIN X20Cr13 relative to DIN USt34-2. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

DIN USt34-2
standard
DIN
DIN X20Cr13
standard
DIN

What else is in Engineering Database

Related comparisons

View each material